NYLENE PX1719 |
|
TECHNICAL DATA SHEET |
General Description |
- Highly impact modified nylon 6 resin. PX1719 has very low stiffness for a nylon type resin
- Can be processed by either injection molding or extrusion
- Suitable for clips, fasteners, and also tubing and profiles, or any other uses where high impact resistance and maximum flexibility are required
Properties
Physical Properties |
Test Method |
Units |
Dry as Molded |
---|---|---|---|
Mechanical Properties | Test Method |
Units |
Dry as Molded |
Tensile Strength | D638 |
psi MPa |
9,000 (62) |
Elongation at Break | D638 |
% |
250 |
Flexural Modulus | D790 |
psi MPa |
95,000 (655) |
Notched Izod @ 23 °C | D256 |
ft. lb./ in. J/m |
16.0 (855) |
Thermal Properties | Test Method | Units | Dry as Molded |
DTUL @ 455 kPa | D648 |
°F °C |
285 (141) |
Melt Point | D3418 |
°F °C |
420 (215) |
All values are for dry as molded specimens. The data set forth herein has been carefully compiled by Polymeric Resources Corporation. Values shown are typical properties and are not for specification. Since processing variables will affect properties, the reproducibility of our data in a customer's facility is not guaranteed. There is no warranty of any kind either expressed or implied, applicable to the use of this information, and the user assumes all risk and liability in connection therewith.
Issued: 2009/09/23